Estado de Disponibilidad: | |
---|---|
Cantidad: | |
Material: aleación 825/n08825, TP316/L, TP304/L, S32205, S32750, aleación 400/n04400, aleación 625/n06625
Paquete: carrete de madera o hierro
![]() | ![]() |
Calificación | C Max | Si Max | Mn Max | P Max | S Max | Cr | NI | Mes | Ti | N max | CU Max | Nótese bien | Al Max | CO Max | Zr | Fe max | Tu | Virginia |
Aleación 600/n06600 | 0 | 1 | 1 | - | 0 | 14-17 | ≥72 | - | - | - | 1 | - | - | - | - | 6-10 | - | - |
Aleación 601/n06601 | 0 | 1 | 2 | - | 0 | 21.0-25.0 | 58-63 | - | - | - | 1 | - | 1.0-1.7 | - | - | - | - | - |
Aleación 625/n06625 | 0 | 1 | 1 | 0 | 0 | 20-23 | ≥58 | 8-10 | <0.4 | - | - | 3.15-4.15 | ≤0.4 | - | - | 5.00 resto | - | - |
Aleación 718/n07718 | 0 | 0 | 0 | 0 | 0 | 17.0-21.0 | 50.0-55.0 | 2.8-3.3 | 0.65-1.15 | 0 | 0 | 4.75-5.5 | 0.2-0.8 | 1 | - | - | - | - |
Aleación 800/n08800 | 0 | 1 | 2 | - | 0 | 19-23 | 30-35 | - | 0.15-0.60 | - | 1 | - | 0.15-0.60 | - | - | ≥39.5 | - | - |
Aleación 800H/N08810 | 0.05-0.10 | 1 | 2 | - | 0 | 19-23 | 30-35 | - | 0.15-0.60 | - | 1 | - | 0.15-0.60 | - | - | ≥39.5 | - | - |
Aleación 825/n08825 | 0 | 1 | 1 | - | 0 | 19.5-23.5 | 38-46 | 2.5-3.5 | 0.6-1.2 | - | 1.5-3 | - | 0 | - | - | ≥22 | - | - |
Calificación | Propiedad física | |||
Ys | TS | El. | media pensión | |
Aleación 600/n06600 | 205-345 | 550-690 | 35-55 | ≤185 |
Aleación 601/n06601 | 240-300 | 600-650 | 30-35 | ≤220 |
Aleación 625/n06625 | ≥345 | ≥760 | ≥30 | ≤220 |
Aleación 718/n07718 | ≥550 | ≥965 | ≥30 | ≤363 |
Aleación 800/n08800 | ≥210 | ≥500 | ≥35 | - |
Aleación 800H/N08810 | ≥180 | ≥450 | ≥35 | - |
Aleación 825/n08825 | ≥220 | ≥550 | ≥30 | ≤200 |
1. Transferencia de gases y líquidos utilizados para calefacción, enfriamiento y una variedad de otros fines.
2. Equipo médico.
3. Energía solar.
4. Fontanería.
5. Manifes de gas.
6. Condensador de superficie de vapor.
Material: aleación 825/n08825, TP316/L, TP304/L, S32205, S32750, aleación 400/n04400, aleación 625/n06625
Paquete: carrete de madera o hierro
![]() | ![]() |
Calificación | C Max | Si Max | Mn Max | P Max | S Max | Cr | NI | Mes | Ti | N max | CU Max | Nótese bien | Al Max | CO Max | Zr | Fe max | Tu | Virginia |
Aleación 600/n06600 | 0 | 1 | 1 | - | 0 | 14-17 | ≥72 | - | - | - | 1 | - | - | - | - | 6-10 | - | - |
Aleación 601/n06601 | 0 | 1 | 2 | - | 0 | 21.0-25.0 | 58-63 | - | - | - | 1 | - | 1.0-1.7 | - | - | - | - | - |
Aleación 625/n06625 | 0 | 1 | 1 | 0 | 0 | 20-23 | ≥58 | 8-10 | <0.4 | - | - | 3.15-4.15 | ≤0.4 | - | - | 5.00 resto | - | - |
Aleación 718/n07718 | 0 | 0 | 0 | 0 | 0 | 17.0-21.0 | 50.0-55.0 | 2.8-3.3 | 0.65-1.15 | 0 | 0 | 4.75-5.5 | 0.2-0.8 | 1 | - | - | - | - |
Aleación 800/n08800 | 0 | 1 | 2 | - | 0 | 19-23 | 30-35 | - | 0.15-0.60 | - | 1 | - | 0.15-0.60 | - | - | ≥39.5 | - | - |
Aleación 800H/N08810 | 0.05-0.10 | 1 | 2 | - | 0 | 19-23 | 30-35 | - | 0.15-0.60 | - | 1 | - | 0.15-0.60 | - | - | ≥39.5 | - | - |
Aleación 825/n08825 | 0 | 1 | 1 | - | 0 | 19.5-23.5 | 38-46 | 2.5-3.5 | 0.6-1.2 | - | 1.5-3 | - | 0 | - | - | ≥22 | - | - |
Calificación | Propiedad física | |||
Ys | TS | El. | media pensión | |
Aleación 600/n06600 | 205-345 | 550-690 | 35-55 | ≤185 |
Aleación 601/n06601 | 240-300 | 600-650 | 30-35 | ≤220 |
Aleación 625/n06625 | ≥345 | ≥760 | ≥30 | ≤220 |
Aleación 718/n07718 | ≥550 | ≥965 | ≥30 | ≤363 |
Aleación 800/n08800 | ≥210 | ≥500 | ≥35 | - |
Aleación 800H/N08810 | ≥180 | ≥450 | ≥35 | - |
Aleación 825/n08825 | ≥220 | ≥550 | ≥30 | ≤200 |
1. Transferencia de gases y líquidos utilizados para calefacción, enfriamiento y una variedad de otros fines.
2. Equipo médico.
3. Energía solar.
4. Fontanería.
5. Manifes de gas.